Re: [MW:25634] LTCS PQR

In case you use process with active gas of flux you have to perform a chemical analysis to determine the A no

2016-10-29 18:28 GMT+03:00 Patel Vivek <vivekpatel1303@gmail.com>:

Possible... But keep dash(-) in A number in both WPS & PQR......custom undiluted weld metal....but they have to comply your other mechanical requirements....


On 29-Oct-2016 8:02 AM, "mmm" <mustaqnk@gmail.com> wrote:
Dear Experts,

Base material  : ASTM A333 GR.6 to A350 LF2 CL 1 or
 P.No 1 & Group No.1 to P.No. 1 & Group No.2
  Pipe 8'' Sch 20 & WN Flange 8'' Sch 20, Impact Test : - 46 ⁰C

Code-ASME B31.3
 
GTAW- ER80S-Ni1 and A#10

SMAW-E7018-1 and A# 1

1) is it possible that we can have different WELD CHEMISTRY A #1 and A#10 in the same PQR please clarify?


Regards
mmm

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/95a556c3-0e66-4ecc-bce5-1683debfa601%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFOZxBiewyrMiepAe95017tuoD04nfKMGk_TSEahRHiMsg%2BQEA%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40BazPMbaWZt%3DOhhHfh%2Bor2n_Sbk9yzqGVPmOFuoz2op6A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...