Wednesday, October 26, 2016

Re: [MW:25600] Regarding electrode for dissimilar base metal

It is not Cast Iron, It is Carbon Steel casting with high carbon. U can use E7018-1 with preheat and post heating

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Tue, Oct 25, 2016 at 5:02 PM, Vivek Pandey <vivek.pande06@gmail.com> wrote:
Dear Sir,
I come across critical situation of welding with cast iron to carbon steel plate.cast iron Material IS2707 GR1 to SA 516 GR 70 or SA 36 (plate).

Following chemical composition of cast iron:
Carbon: 0.472%,Mn: 0.891%,Si: 0.566%,P: 0.04%,S:0.04%

  Kindly suggest us SMAW welding electrodes and preheat and post heating requirement during welding of same dissimilar base metal.

Regards,
Vivek Pandey

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANCwoYnG1zC_osifwAB%2BSS_O5r%3DMjN1s8Fj%3DHLeVT7Wvti%3Dngg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNMvjC_kg%3D50nTN2Lgu%2B65KhQkWey4QSzFwj5P2M%3DaC%3DQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...