RE: [MW:25579] regarding under cut and concavity in welder qualification

QW-302.4 requires a visual examination per QW-194.  QW-194 requires complete joint penetration and complete fusion.  Concavity would be considered not complying with the requirement for complete joint penetration.  However, undercut within manufacturers quality requirements would be acceptable as per Interpretation IX-01-03.

 

 

Enjoy.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of anil kumar
Sent: Thursday, October 20, 2016 10:35 AM
To: Materials & Welding
Subject: [MW:25576] regarding under cut and concavity in welder qualification

 

Dear Sir,

 

      1.please provide me acceptance values for under cut and concavity for welder qualification(asme sec9).

       2. is it true that as per ASME sec 9 undercut is not consider for welder qualification.

 

 

Thank you

Anil Kumar

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/809ada97-27ef-4aad-8361-fa451623ec39%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...