Re: [MW:25561] Hydrostatic leak testing

if not a sensitive test is not required you may go ahead. For sensitive leak test check 345.8.
However, is up to the Engineering to determine if a sensitive leak test is required.

2016-10-17 14:07 GMT+03:00 'prem_nautiyal26' via Materials & Welding <materials-welding@googlegroups.com>:

Dear all

Vendor has offered piping spool for hydrostatic test after painting.

Code of construction is ASME B31.3. Category M fluid service.


Vendor argues that as per ASME B31.3 clause 345.3.1 all joints may be primed and painted prior to leak testing.

However same clause also mentions that all joints Welds shall be left exposed for examination during leak testing which is contradictory. 

Nothing is mentioned in hydro test procedure about painting.

How to accept ?

Regards 

Prem  Nautiyal 
9769316004



Sent from my Samsung Galaxy smartphone.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7jn1h51k7qvstcl9oslvcb88.1476701958103%40email.android.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40AQdOV5gpx45qojHYOMT_9W3OhYsPj-7umr%3DBM2vu2_%3Dw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...