Monday, October 17, 2016

Re: [MW:25558] do we need seperate wps for repair

Dear,

The statement in the clause 328.6 say, the grove shape of repair weld may be different from the original weld joint.

Regards,
CH V Ramana
BVIL




On Monday, 17 October 2016 10:30 AM, 'prem_nautiyal26' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Hi

You only need to prepare the repair procedure wherein your production WPS will be referred.

Regards

Prem Nautiyal 





Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: anil kumar <anil.qcqa@gmail.com>
Date: 17/10/2016 09:35 (GMT+05:30)
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25551] do we need seperate wps for repair

Hi,

       Do we need separate wps for repair or the wps we used in production will be sufficient as per ASME B31.3,
and using the  PQR which used in production , can I qualify repair wps.

Thank you
ANIL KUMAR
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/083fabc6-d945-43b4-ab2b-a50ffd3cec46%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/i71n4jfcxfi8um4xc7oq34qd.1476680174697%40email.android.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...