Dear Friend,

2" Weldolet od will be more than 73mm and section 9 talks about OD.
My interpretation says we can weld , is there any code case or interpretation file number regarding same, if any of you arr aware please share.

Regards

Vikas


On 16 Oct 2016 10:05 a.m., "anthony chundal" <anthony.chundal@gmail.com> wrote:

Dear all,

Thickness of both base materials also shall be considered as per Qw202.

Regards,
Anthony.


On Oct 15, 2016 19:32, "Patel Vivek" <vivekpatel1303@gmail.com> wrote:

Dear vikas,

You have to qualify welder in 2 inch to weld that weldolet on 24 inch pipe....

Regards,
Vivek


On 15-Oct-2016 5:50 PM, "Vikas Waghmare" <vikas.waghmare08@gmail.com> wrote:

Dear all,

I want to weld 2inch weldolet to 24inch pipe, my doubt can i use welder qualified as per section 9 with diameter range 73mm and above to weld 2 inch weldolet whose OD is above 73mm.
Second doubt how much weld i need to deposit on weldolet to run pipe connection if code of construction is asme B31.3, i think it should be minimum thickness of branch or run pipe thickness and then make fillet. Or is it needed to deposit weld upto bevel end then a fillet.

Regards

Vikas

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BCgecnc-uScigVNxcd15GJQmb8ZhT-SWKO2eoFX%2BJhg7%2Bkpyw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFOZxBj6SVzj%2B7RFXREdsRGSqgM_5Xm2MvR8Dr3Z9O-sD0gr2w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp-Y8OUuuuHgt4-LD4%3DYfEe8TQcLUBVjqOnXbsAB8s3apA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BCgeck7VQfFCXvCdgg2%3D5QPZKb0voqs862boMCr%3DWqVQeUunQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...