Friday, October 14, 2016

Re: [MW:25544] API 6A, DESIGN VERIFICATION REPORT CLARIFICATION

Hi,
That EE - sour service with SS internal parts.
NL - No Limit of H2S Concentration.
Thanks and Regards,
Rajagopal Kannan


On 14 Oct 2016 1:36 p.m., <mylsamy.qc@gmail.com> wrote:
Dear raj,
Can you please specify where is given N and L value in API and what is the component are you looking for?

Sent from my iPhone

On Oct 14, 2016, at 8:25 AM, 'raj susi' via Materials & Welding <materials-welding@googlegroups.com> wrote:

<20161014_121208.jpg>
Dear Prakash

Thanks for your reply.
My question here is the - 
when the design parameter is -20 deg F to 250 deg F, can the Material class be only -50 deg F to 180 deg F?
-50 deg F is more than -20 deg F, FINE for minus degree service.
But 180 deg F is less than 250 deg F, should the material temperature be equal or greater than Design? this is my question in the previously attached report. 

regards
raj


On Thu, 13 Oct, 2016 at 17:16, Prakash Gotimukul
 Who gave the design parameters? If given by client then, design it to that. Not the service parameters.

Rgds
Prakash Gotimukul
AIS, Consultant ASME/ISO/PED/IBR

On Mon, Oct 10, 2016 at 2:09 PM, 'raj susi' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Experts



Good day to all.
I reviewed a DVR as per the attached, 

Design parameters:- 
Max working pressure 5000 psi.
Design temperature -20 deg F to 250 deg F.
Service Sour 
Service Material class EE NL.

Here, SERVICE of the product is as below,
EE denotes sour SERVICE=SAME AS DESIGN REQUIREMENT.
N denotes -50 to 140 deg F. & L denotes -50 to 180 deg F.
So we can combine and get NL as -50 to 180 deg F. NOT SAME AS DESIGN REQUIREMENT.
MY QUESTION IS -
DOES THIS PRODUCT SERVICE MATCH WITH DESIGN REQUIREMENT? 
Do we need to change the lower/higher temperature limit of design/service or it can be the same?

Please give your valuable. comments on this subject.

Regards 
Raj 


<20161009_132033.jpg>


--
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
To post to this group, send email to materials-welding@ googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/ msgid/materials-welding/ 539457555.1002882. 1476094177885%40mail.yahoo.com .
For more options, visit https://groups.google.com/d/ optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4qJdz%3DAZaZaj89cNkRRFc0VvbhDqYPq6VWbiBm-YSMUNrQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1412316375.105633.1476419139756%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
<20161014_121208.jpg>
<20161009_132033.jpg>

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/EB1F009E-D0DB-4B35-B836-36B390C807E6%40gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD3oVpAKg9VDr7sXV%2BpxgPFD%3Dxw7ttec_WuCDHoOXV6g4i%3DKkA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...