Hi,
PMI for alloy material(T11,22,91,etc.,) only to identify Possitive Material. If you want to verify chemocal properties of CS then you go for X-ray Fluorescence Spectrometer.
 
Thanks& Regards,
 
(Karthik)
QA/QC Manager 
CMI-Thai Services Co.,Ltd. 
50/35 Sermsuwan Road,Tambol Maptaphut 
Amphur Muang Rayong,Rayong 21150
Thailand
www.cmi-services.com 
Tel : +66 38 691 390-2 ext.103 
Fax : +66 38 682 338 
Mobile: +66 892512282 
E-mail : karthikeyan@cmi-services.com
               Karthik6684@yahoo.com


On Friday, October 14, 2016 10:51 AM, Mani <dmm.sgnp@gmail.com> wrote:


Hi all,

  Pls advice when & why we required to do PMI for carbon steel materials?

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6f241415-48b9-47c3-919a-79c17570ccb0%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...