Friday, October 14, 2016

Re: [MW:25540] API 6A, DESIGN VERIFICATION REPORT CLARIFICATION

Dear raj,
Can you please specify where is given N and L value in API and what is the component are you looking for?

Sent from my iPhone

On Oct 14, 2016, at 8:25 AM, 'raj susi' via Materials & Welding <materials-welding@googlegroups.com> wrote:

<20161014_121208.jpg>
Dear Prakash

Thanks for your reply.
My question here is the - 
when the design parameter is -20 deg F to 250 deg F, can the Material class be only -50 deg F to 180 deg F?
-50 deg F is more than -20 deg F, FINE for minus degree service.
But 180 deg F is less than 250 deg F, should the material temperature be equal or greater than Design? this is my question in the previously attached report. 

regards
raj
+65 98489500





On Thu, 13 Oct, 2016 at 17:16, Prakash Gotimukul
 Who gave the design parameters? If given by client then, design it to that. Not the service parameters.

Rgds
Prakash Gotimukul
AIS, Consultant ASME/ISO/PED/IBR
 Mob:+97152 979 5678

On Mon, Oct 10, 2016 at 2:09 PM, 'raj susi' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Experts



Good day to all.
I reviewed a DVR as per the attached, 

Design parameters:- 
Max working pressure 5000 psi.
Design temperature -20 deg F to 250 deg F.
Service Sour 
Service Material class EE NL.

Here, SERVICE of the product is as below,
EE denotes sour SERVICE=SAME AS DESIGN REQUIREMENT.
N denotes -50 to 140 deg F. & L denotes -50 to 180 deg F.
So we can combine and get NL as -50 to 180 deg F. NOT SAME AS DESIGN REQUIREMENT.
MY QUESTION IS -
DOES THIS PRODUCT SERVICE MATCH WITH DESIGN REQUIREMENT? 
Do we need to change the lower/higher temperature limit of design/service or it can be the same?

Please give your valuable. comments on this subject.

Regards 
Raj 


<20161009_132033.jpg>




--
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
To post to this group, send email to materials-welding@ googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/ msgid/materials-welding/ 539457555.1002882. 1476094177885%40mail.yahoo.com .
For more options, visit https://groups.google.com/d/ optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4qJdz%3DAZaZaj89cNkRRFc0VvbhDqYPq6VWbiBm-YSMUNrQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1412316375.105633.1476419139756%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
<20161014_121208.jpg>
<20161009_132033.jpg>

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...