Hi All,
Hope you all doing well.

Test Code BS EN ISO 9606-1
Client requested to carry out WPQ  test on roundbar 60mm dia.

I feel we need to weld 3nos. Joint of 60mm dia so that we achieve 180mm exam length (reqd 150mm)

Contractor want to weld only one joint saying consider it is 2"pipe.

Kindly advise with standard reference.

Thanks

Aly

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOenW4g1_JpCz%2BSYoeKpDEmZYydvgbnhi7Ony_WQxTvvXS7jcg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...