[MW:25573] why fluactuation in my tensile test graph

Dear  Expats,

the attached graph is that of a tensile test carried out on 304 stainless steel rod of 12mm diameter. the steel is heat treated and quenched in water. please can anyone help explain why i have fluctuation in the graphs ( i mean the series of sharp decline in stress as shown in the graph)

kindly help....

Thanks for sharing.

Patrick Oghate

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6ad5ff12-7788-4374-8a67-5cf97ca46296%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...