Dear all,

I want to weld 2inch weldolet to 24inch pipe, my doubt can i use welder qualified as per section 9 with diameter range 73mm and above to weld 2 inch weldolet whose OD is above 73mm.
Second doubt how much weld i need to deposit on weldolet to run pipe connection if code of construction is asme B31.3, i think it should be minimum thickness of branch or run pipe thickness and then make fillet. Or is it needed to deposit weld upto bevel end then a fillet.

Regards

Vikas

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BCgecnc-uScigVNxcd15GJQmb8ZhT-SWKO2eoFX%2BJhg7%2Bkpyw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...