Re: [MW:25310] Welding

Hi

Based on my experience for tank fabrication, the next day welding will be allowed, for piping and pipeline if it is higher thickness/nig bore line pipes/non sour will be allowed after competition of 70% welding and the same will be discussed with Client for acceptance prior to implementation.

For sour service piping and pipeline delayed will not be permitted, delayed PQR will be conducted for demonstration/destructive testing. Please note that there will be an additonal NDT methods will be carried out on the production welds for Clent acceptance.

With kind regards
Govindan Perumal

On 20 Aug 2016 05:16, "richard burthon" <richardburthon@gmail.com> wrote:
Dear All,

Could  welding to be continued tomorrow but WPS/PQR is qualified without overnight,,?please give me any reference for this case

regards

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/309dc329-65dd-4bf5-9e45-c8718e91a08e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9esfL6gE44n8gxWJ-2jBaO8cXmDM9O%2BctVHdOr1imG56A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...