Hi Kumar

Surface Profile as per Client/project specification is 30 - 70 microns. Profile range was specified by the paint manufacturer will not be considered, always Client requirement shall only be followed.

After blasting the surface profile shall be within the above mentioned range, its not mandatory that the surface profile should be 70 microns minimum.

Alternativly the profile will be also checked by profile gauge (elco meter).

Explain to Client representative for acceptance.

With kind regards
Govindan Perumal

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9fjEr1tHBOCjB%3DVXu%3DDWnmbJHXfU_5LfGvYNTW_eo13fQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...