Tuesday, August 23, 2016

Re: [MW:25302] Post Forming Heat Treatment of SS316L Dish

Hi all,
Refer attached discussion on this topic...

Aly

On Tue, Aug 23, 2016 at 9:41 AM, Mhaskar Aly <mhaskar.aly@gmail.com> wrote:
Dear Mr. Prasad,
What if Fibre elongation exceed 20% (for SS316L Dish), PFHT required or not; please provide Code reference.
Thanks
Aly

On Sun, Aug 21, 2016 at 4:07 PM, Prasad Ghanekar <prsgne@gmail.com> wrote:

PFHT is not mandatory as per code.
Some client specify PFHT as solution annealing if hardness after forming is more than 22 HRC

PVG

On 21 Aug 2016 17:08, "A Ahmed Ahmed" <1aajtak1@gmail.com> wrote:
Dear All,

Code: ASME SEC VIII-1

Post forming Heat Treatment of Dish...

MOC: SS316L

Design Temp 85°C

Fibre Elongation: 3.6%

UHA-44 table does not show values of Fibre elongation..

Is PFHT required for this dish.

Kindly advise

Ahmed

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BL7tiPwcXf8BVFYiF_b%2BCF3jdfsjhVdQGAyK-FfvAhpWOZDOQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEi5r3YaX6d%3D%2BpdHEZ_A6kh4Z4t6WB0MnwpT2KGKi2VGUuiGUQ%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOenW4gSv%3DUh6pjT%3DXLoYkXe3sKrYzBpTn9TPLOk1Ap7xH2nWg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...