Monday, August 22, 2016

Re: [MW:25291] STUD AND BOLT


For Process Piping B31.3,  335.2.3, Bolts should extend completely through their nuts. Any which fail to do so are considered acceptably engaged if the lack of complete engagement is not more than one thread.

Regards,
Sajeev

On Sat, Aug 13, 2016 at 6:47 AM, Sundaraj Anish <anishsundaraj@gmail.com> wrote:

Dear experts,

I have a query and looking  for earliest  response

How many threads should protrude beyond the nut?

 minimum 3 threads and maximum how many threads ?

Awaitng for your  response

Thanks & regards

Anish S 

Engineer-QA/QC

Mott MacDonald Pvt Ltd

Hassan

Mob: +91 9442938358

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtc4G5ccCSktoX3iRe_3WOgjJgiZUXPo6Jc3HuW%3D4Oa8YMTAQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANSvUP0QTA67YgecmcaM3Av8BqPFAoO5c-5_qr-2O14Fpkj9kw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...