Dear Mustaq,

Since you mentioned B.31.3  for the proper consumable selection , please specify the process.
is it  GTAW+SMAW   combination  or full SMAW?
 

Best Regards,

JIJILAL K.M. 



On 16 August 2016 at 00:45, 'c sridhar' via Materials & Welding <materials-welding@googlegroups.com> wrote:
For CS, minimum min. UTS values of consumable selected  must be just above the 
values of min. base metal. Chemistry is not a criteria as it may differ from base toweld chemistry.

For your 106 Gr. B pipe,it could be,

1. E 6013 for root, filler cap  or 
2. E 6010 for root and E 6013 for F & C. or
4. E 6013 for root and E 7018 for F & C  or
4. E 7016 for root and E 7018 for F & C (used in shipyards) or
5. E 7018 throughout.

1 & 2 are common in plant piping. 

For AS & SS , chemistry of base mental is the criteria and not UTS values.

Trust it is useful to you.
Sridhar.
---------------------------------------------------------------------------------------------------






From: 'anand gupta' via Materials & Welding <materials-welding@googlegroups.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>; Mustaq Ahmad <mustaqnk@gmail.com>; Materials & Welding <materials-welding@googlegroups.com>
Sent: Tuesday, 9 August 2016 9:07 PM
Subject: Re: [MW:25236] Basic rule for selection of consumable for piping

Dear
minimum base matel tensile and chemical composition is required or higher will acceptable. 

A p gupta
baroda


On Tue, 9 Aug, 2016 at 18:38, Mustaq Ahmad
Dear experts

I am working as QC-ENGINEER, as I am preparing wps/pqr 1st time,I need some guidance regarding consumable selection like what are criteria to be considered,
Example for b31.3 and  section IX is the code carbon steel is material A106grB pipe. In this how we select from sectionII part C

Regards
Mustaq

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0568c66f-2bc8-4c9a-8794-b82f6a6d137b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1802857053.10716575.1470757039517.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1102423112.13169676.1471283143333.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHgZw-KmoMg40tBDTrUOZX8_gSSAh0izdH9x%3DmdyN56LJg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...