Monday, August 15, 2016

Re: [MW:25258] STUD AND BOLT

Dear,

As per api standard it shall be 1 thread only.Pls check project specs.

Regards
Dinesh

On Aug 15, 2016 7:39 AM, "Thulasi Das" <prtdas74@gmail.com> wrote:
Hi Sundaraj,

Maximum three threads.!!!

Regards.

P.R.T.Das.


On Sat, Aug 13, 2016 at 9:17 AM, Sundaraj Anish <anishsundaraj@gmail.com> wrote:

Dear experts,

I have a query and looking  for earliest  response

How many threads should protrude beyond the nut?

 minimum 3 threads and maximum how many threads ?

Awaitng for your  response

Thanks & regards

Anish S 

Engineer-QA/QC

Mott MacDonald Pvt Ltd

Hassan

Mob: +91 9442938358

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtc4G5ccCSktoX3iRe_3WOgjJgiZUXPo6Jc3HuW%3D4Oa8YMTAQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BC4rf2fooD2LH%3DKOMUONVWbAO-ZvKCJyFv6wDtinfPDFBMvqQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrW8%2BtCDAD_6Z0f28zy9DRDFZMKwqUZD6P17sPd2hANd-A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...