RE: [MW:25255] Problem in welding tube to tube sheet welding

Dear Chandan Sharma,

The leaks in your tube bundle appears to be from the cracks in the Tube/Tube sheet welds. Please look at your fabrication details for the tube bundle. The cracking could be caused by the expansion of the tubes while in service.  

A thorough investigation into the Manufacturing process will be needed before attempting a repair procedure.

Regards

George V Aliyattukudy

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of chandan sharma
Sent: Friday, August 12, 2016 11:18 AM
To: materials-welding@googlegroups.com
Subject: [MW:25245] Problem in welding tube to tube sheet welding

 

Dear Experts,

 

We are facing problem of leakage during service condition in heat exchanger. Leakage are coming in the  tube to tube sheet welding in service condition. Attached are the reference photos

Details are defined below,

Construction code – ASME SEC-VIII Div-1 and Div-2

Material – Tube Sheet - SA 240 UNS 31803

Tube   - SA789 UNS 31803

Filler – ER2209

  Allowable Temperature – Shell –    +180 / -30 C, Pressure- 1 bar /FV

   Allowable Temperature-   Tube- +200 /+10 C, Pressure 10 bar

                               MDMT -0 C

Service Media –            Shell – Methanol + LIBR

Tube – Thermal oil

 

Let us know why such failure occurs and preventive actions

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTWUJL8WSL77tHp8HGSVH7pYZfm4Oe3-xzmBHntE3n5aaKpYQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...