Re: [MW:25254] STUD AND BOLT

Pending Construction Code ASME B31.3  Parr. 335.2.3 Bolt Length. Bolts should extend completely through their nuts. Any which fail to do so are
considered acceptably engaged if the lack of complete
engagement is not more than one thread.






De: materials-welding@googlegroups.com <materials-welding@googlegroups.com> en nombre de Harish Kannepalli <harishkannepalli@gmail.com>
Enviado: sábado, 13 de agosto de 2016 12:38 a. m.
Para: materials-welding@googlegroups.com
Asunto: Re: [MW:25253] STUD AND BOLT
 

Minimum length shall be equal to diameter of bolt


On Aug 13, 2016 08:59, "Sundaraj Anish" <anishsundaraj@gmail.com> wrote:

Dear experts,

I have a query and looking  for earliest  response

How many threads should protrude beyond the nut?

 minimum 3 threads and maximum how many threads ?

Awaitng for your  response

Thanks & regards

Anish S 

Engineer-QA/QC

Mott MacDonald Pvt Ltd

Hassan

Mob: +91 9442938358

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtc4G5ccCSktoX3iRe_3WOgjJgiZUXPo6Jc3HuW%3D4Oa8YMTAQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE4SttHQXAxoDTS0Skc%3DA1CYrYfz4jAVeSV2hbf1VQHiohRa%2Bw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...