Dear Experts,
Just a query regarding PQR & WPS generation. the project spec. calls
to follow PQR &
WPS according to Sec. IX for construction of pressure vessels ( MOC-
SA 516 Gr. 70 N). complying to to ASME Sec. VIII Div.1.
Also the allied base frame structures ( skid frame) too with the above code.
The work had been assigned to 2 diff. sub-cons & one of them made PQR
& WPS according to AWS D1.1 in order to use the welding of
structures. this was done due to the queries & enforcing of Main cont.
engineer though spec. calls for Sec. IX !
But here, one sub-con is unable to provide AWS D1.1 PQR & WPS due to
practical difficulties & says both don't have much differences.
Our doubt is that, once the mecahnical integrity of the intended weld
is proven with Sec.IX PQR, then what is the necessity to call for AWS
D1.1 PQR, WPS etc...?
your valuable feedbacks are highly appreciated.
Thanks in advance,
kumar.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALuBtp9nsuxHpxS7vgbrJ7sW9LishaWqsoAVZiMmp9rwny3rWw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...