Dear Brothers ,

      I did Pickling and Passivation for SS tank , 

Brand Name : 

1) Pickling : Avesta Pickling Spray 204
2) Passivation : Avesta Finish One Passivator 630

Actually Now i am Facing problem of Molten Slag  Melt at settlement at Shell Plate , Please Refer Attachment file 

My Question Is : If the  Molten Slag not Removed From shell course means ,  will affect any  at Future corrosion  at shell area or Not , According to ASTM A380



Please advice me , I am waiting for your Valuable answer 

Best regards
Sankar.k
Welding Inspector 
Enka-Iraq

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ed2987e5-5638-49d7-8137-e13a757eb959%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...