Hi KCR,

 

You need to repeat the hydro test following. Please see Sec-VIII, DIV-1, UG 99 (a) (1). Also see the following discussion in Eng Tips discussion forum also:- http://www.eng-tips.com/viewthread.cfm?qid=212412.

Depending on the design codes there could be some relaxations.

 

However the default rule, is to repeat the hydro test after any further welding.

 

Thanks.

 

 

Pradip Goswami, P.Eng,IWE

Welding & Metallurgical Engineering Specialist ,
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgoswami@quickclic.net

pradip.goswami@gmail.com

H-905-6799677, 905-9631505

C-905-9793232

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of k c
Sent: Friday, August 26, 2016 12:34 AM
To: materials-welding@googlegroups.com
Subject: [MW:25316] Post Hydro test welding of Section VIII Div 1 pressure vessels REg.,

 

Dear All

 

Can any body suggest code required testing, for the welding done after hydro test.

 

this welding is done on hydro tested shell,  after hydro test. Code vessels and U Stamping required.

 

Best Regards

K C R

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL9TLdcUnFv1zzSgYJ82nqzg7L72P3QdihuNtYKLMSJjaOZDXA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...