Monday, August 22, 2016

[MW:25287] Diffrence between Cr content range in casting and forge SS316

Dear Experts
Good day!!!

I'll highly appreciated if you share your valuable ideas regarding reason for difference between Cr content range in A351 CF8M and A182F316 which is 18-21% and 16-18% respectively.

Regards,
H.Nikdin

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BLU405-EAS243C25FF6CC7E1A871214F39EE80%40phx.gbl.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...