Dear Experts,

Greetings for the day.

I have a query regarding surface profile of CS for blast surfaces of
pressure vessels, piping & structural.

Client spec. calls for- the surface profile for CS shall be 30-70
microns as measured with a replica technique (typically testex tape
used in accordance with NACE RP 0287).

But the paint manufacturer allows for 30-85 microns grade fine to
medium G; Ry 5 (ISO-8503-2). with SA 2.5 surface roughness.

Here, it is obvious that on practical grounds, it would be somewhat
difficult to achieve a maxm. 70 microns finish as it may go beyond
also ( which is foreseen by the paint manufacturer). but client is
strict for 70. how could we convince them in this regard.

Thanking all in advance,

Kumar.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALuBtp-YJXXgGoE_ouognT__KVnri%3DKHGOt_O%2BwZJ-8XTV7ruA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...