Wednesday, August 10, 2016

[MW:25236] Multiple welders on single production joint

Dear experts,

I have a query n looking  for earliest  response
I had welders qualified on 1/2" OD with 7.46mm thk
Now we had a production joint of 2" OD with 8.75mm thk, which is required  to be    done with full tig

Now the question is, Can we engage two 1/2" qualified welders to weld 8.75mm thk??
Is there any clause in sec.ix for having two welders on single production joint to cater excess thk??
Or should we go for separate qualification using 2 welders on single test cupon??
Plz update me the clause no. If it is allowed

Awaitng for your quick response

Thank you all

Regards
Prasad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKgcArTBn1q8qXcabJnNuhU2zCFy3p6H5LJMOsvZJv6jS07cXg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...