Tuesday, January 5, 2016

Re: [MW:24054] repair joint

Once you did the repair you have to do RT to check whether the repair has been done or not if it is accepted RT than only you can release the joint.

Sent from my ASUS


-------- Original Message --------
From:"Eng.Mahmoud kamel"
Sent:Mon, 04 Jan 2016 21:18:19 +0530
To:"M.W"
Subject:[MW:24052] repair joint




Dear all ,

one joint cut out due to repair  in RT and welded again by another welder .RT second time mandatory or not .

please need your reply with support code or document from ASME 

best regards
mahmoud

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ppm2fxxwfsjswh70ix0qfbsa.1451977384957%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...