Dear Sir,

You have to study the properties of painting system applied. Demonstrate the ultrasonic wave is passing through the painting or not. If it passed through the painting without any disturbance then the procedure could be written and get approval from Level II and follow.



Thanking You.

With Warm Regards,

Muthu Barathi P.
Mobile : +919967300544 (Only message )
Mobile No. +965 50989210 (KUWAIT) after 8PM


From: Mohd Siraj <mohd52100@gmail.com>
Sent: Sun, 03 Jan 2016 14:04:41
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:24037] UT in painted condition
its hard coating or painting??

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/60a73a02-0507-4b6f-a994-f17aba444f69%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1451810081.S.4683.13686.f5-224-110.1451897335.18195%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...