Yes, you can do only for thickness measurement.
Thanks & Best Regards,
Kareem.
On Saturday, 2 January 2016 3:21 AM, "erbsmn@gmail.com" <erbsmn@gmail.com> wrote:
Hai,
whether UT can be done in painted condition??
Kindly share your opinions..
Sent from my iPhone
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9B05F42A-27B9-4AB3-8A29-7985C7C00EFA%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
whether UT can be done in painted condition??
Kindly share your opinions..
Sent from my iPhone
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9B05F42A-27B9-4AB3-8A29-7985C7C00EFA%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment