YOU CAN USE THE SAID WPS. IT IS ACCEPTABLE
On Tuesday, December 8, 2015 at 8:58:42 AM UTC+5:30, Reddy wrote:
-- On Tuesday, December 8, 2015 at 8:58:42 AM UTC+5:30, Reddy wrote:
Dear expertsAs per sec IXI have an PQR which qualified on 3G(Plate) soQ.1) Can i use that pqr for to weld 3Nps pipe 6g positions welding.or is there any conflict between plate and pipe qualification.If there experts can explain why?Bets regardsreddy.