[MW:24035] RE: 24033] RE: 24027] Hydro test

Dear Friends

 

Per your say a very small drop in pressure - 

Note that a very small is no where acceptable, but there are exceptions that may say " so many drops per minte" etc.

So you need to be very specific

 

N. Singh

 

Maharashtra, India.

 

PLEASE THINK BEFORE PRINTING

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Lakshman
Sent: 02 January, 2016 10:24 AM
To: materials-welding@googlegroups.com
Subject: [MW:24033] RE: 24027] Hydro test

 

Hi friend,

Please elaborate the query with necessary details to look in to that.

 

Thanks & Regards,

Lakshman Kumar B,

9440031459.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Nishanth Km
Sent: Friday, January 01, 2016 12:11 PM
To: materials-welding@googlegroups.com
Subject: [MW:24027] Hydro test

 

Dear experts,

Is pressure drop(very small) acceptable in piping during hydro test beyond temperature variations. Please advice.

Regards

Nishanth

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Ba8N2%2Bez91HCXKpWy%2B-RFqCAgpKOsKs6OjSOOggmxWtcY43Kw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/002901d14519%2493af6760%24bb0e3620%24%40com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone