it will increase strength, inhibitors fine grains

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Mon, Nov 30, 2015 at 7:54 PM, Vishwas Keskar Welding Manager Pune India <vvkeskar123@gmail.com> wrote:
Dear Experts ,

We intend to use SA 516 GR 70 plate - (thickness ranging from  55mm to 100 mm)  for   steam boiler application.
We are getting plates with Niobium content of 0.04 %.
As per SA 20   corresponding table ,the maximum limit for Nb  is 0.02 %
How ever , in the notes of the said Table  the Nb can be increased
What is effect of increase,  in Nb element on boiler drum shell rolling and  welding


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/05cb8aec-9be2-45e2-8d97-57c1b2dae3b7%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOrANXoiLfmy5Lj%2B%2BQjriFLj7U6YTiaNpRJKWgyO9TkTA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

2 comments:

Unknown said...

Can we accept the 0.04% Nb if there is no problem w.r.t. Rolling and welding.

BR said...

refer Note D on Table 1 SA 20

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...