Re: [MW:23500] Test requirements for WPQ of 5F pipe to plate joints as per ASME Sec 9, QW 462.4 (c)

Dear Mr. Dileep,

The test is for Welder Qualification, nothing to worry too much. This test is to check the welder is capable to perform the sound weld or not.

I will request you to check the following:

                    Please check the responsibility from client Std. who can witness the test. If nothing is mentioned no need to involve Laboratory to perform the test, Project Inspection can do the same.


Now I think the joint is Pipe to Plate.
 The specimen for test is mentioned in Figure QW-462.4(c).
Also the test can be done as per attached picture. Just go with the pic get the result.


I think this information will help you, but ultimate is client std., what they are asking for.



On Thu, Sep 17, 2015 at 1:28 PM, Dileep Sankar <dileepsan.08@gmail.com> wrote:
Dear All,

We were asked to qualify the welders for tacking, while the fit-up of pipelines in our current project. The client has specified to use GTAW technique for the tacking and the position to be maintained is 5F, (pipe to plate). The standard I am referring to is ASME 2007 edition.

       i. The test position was determined through QW 132.4 --> specifying 461.6 (e)
       ii. The test specimens were cut out as per QW 462.4 (c) [Page no: 159]
       iii. The tests were determined via QW 181.2 ---> Tests for Fillet welds, performance.
              1. Fracture Test => QW 182.
              2. Macro examination => QW 184.
       
I believe that this much steps which I have taken are correct for my requirement. The Client too has agreed upon these. Here, the macro examination also does not pose any issues, since I am quite sure of how to do it. But, on contacting certain labs here in the localities, which are known for performing Destructive and NDT for WPQ, they informed me that the necessary equipment for performing the Fracture test, is not available with them. But, when I extended my search, I am coming up with more negative answers, which also included that they do not know how to perform the specific fracture test.

On supplying the same query to our client, they are keeping their stand, to perform the tests as requirement, even though they are not providing any ideas for the same. Now I am at a road block, on how to perform the mentioned test.

So, please take this matter into your hands and give me some valuable advice, for which I am already grateful.

With all due regards and thanks in advance,

Dileep Sankar.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f186b0ce-857b-4a12-a461-0faafea15d31%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFnzQg16iQCMnfyKhvAb8qbRCYMzb%2BWCfRY%2BTbCSBjWG_8vizQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...