Re: [MW:23484] WPQR as per EN 15614-1

Definitely You can do but consider thickness range
Eknath

On Sep 15, 2015 4:12 PM, "Vijay Katkar" <katkar.vijay22@gmail.com> wrote:
Dear All,

Need your assistance,

I have qualified WPQR for fillet weld (Plate to Plate) as per EN 15614-1.

Can i use this PQR to weld pipe (15 mm OD) to plate for fillet weld (thickness range is within specified limit)?

Please guide me on this.

Thank you

Vijay Katkar 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP37wrJHuASs4hgSdXXR17aezNU0bkbmBZcVfgC8nuBCMzPWfQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABBYVhJh%3Dipj%3DN%3DT%2BS-HZn4nXWJ7Ma3M%3DJ9Mm9cGG5mZKtuJFA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...