Monday, September 14, 2015

Re: [MW:23476] Using ASME IX WPS for replace with AWS D1.1 structure job

Hello Rahim,

It depends on your client!

Few reputed clients accept ASME Section 09 WPS in place of AWS D1.1.You can convinces your client by referring to API RP 582 - 2nd Edition, Clause 4.

Before approaching your client ,please ensure API RP 582 is applicable for the project.

 

4 General Welding Requirements

4.1 Structural (nonpressure boundary) welding requirements shall comply with either AWS D1.1 or AWS D1.6.

When approved by the purchaser (engineer) welding procedures may be qualified per ASME BPVC Section IX."


Thanks and regards,


Sudhakar.K



On Wed, Sep 9, 2015 at 5:08 PM, mohd firdaus <mohdfirdaus.abdrahim77@gmail.com> wrote:
Dear all,

I have a situation here. We got steel structure job but my AWS D1.1 WPS not covered for this job. It is possible to replace the WPS WITH ASME IX WPS?. My boss told me to sent the STQ request for replace the AWS D1.1 to ASME IX. I don't have any idea for this. Please guide me. Thank you.

Mohd Firdaus Abd Rahim
QA/QC
+60122796361

Sent from my iPhone

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CEC1A20B-5BC3-4448-A2D6-60067EA848D2%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BfZfcPF%3DTSf4F0wt9j6HBL360%3D9Phf8AWAJw1wFq2y97tkF2A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35614] Re: SS FILLER

dear , pl check A number and Gas composition use for ss cant be sutibale same % for duplex., u need to qualified with aditional testing of f...