Re: [MW:23414] Procedure Qualification Hot wire vs Cold wire TIG

is Impact testing required? it will effect other parameters, for e.g QW 409.1 (travel speed and amp are higher in case of hot wire)

On 7 September 2015 at 13:25, FAIRON Luc <luc.fairon@cmigroupe.com> wrote:

I have got a PQR qualified for orbital TIG welding (automatic) with cold wire. Does it qualify for orbital TIG welding with hot wire, all other thinks remaining unchanged ? In my opinion yes, but I am not sure. Applicable construction code is ASME. Welding qualifications are per Section IX.

Regards

 

Luc FAIRON
Welding Engineer

 

 


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubk7YYMvF3GiWQ96OdiLqWN_yRGemiCgATEiwtJGf2hDoQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35725] Dismillar material Welding

Dear experts,  In my Hydro Electric Project  materials using A517Gr.F and A537CL-II.  For A517Gr.F using E 11018M and A537CL-II using E 9018...