Sunday, September 6, 2015

Re: [MW:23408] PWHT requirement for vessel

Hi

As the nominal thickness exceeds 38mm then in my opinion you have to carry out PWHT in-order to relieve the residual stresses, else take the risk of catastrophic failures in service..

Regards

Prem Nautiyal
cell: 9769316004







--------------------------------------------
On Fri, 9/4/15, Prasad Ghanekar <prsgne@gmail.com> wrote:

Subject: Re: [MW:23391] PWHT requirement for vessel
To: materials-welding@googlegroups.com
Date: Friday, September 4, 2015, 12:22 PM

40 mm butt
welds
On 4 Sep 2015 10:19,
"'prem nautiyal' via Materials &
Welding" <materials-welding@googlegroups.com>
wrote:
What is
the max. nominal thickness of weld involved in skirt support
?



Regards



Prem Nautiyal

9769316004



--------------------------------------------

On Mon, 8/31/15, Shadab Ansari <shadabansarialam@gmail.com>
wrote:



 Subject: Re: [MW:23374] PWHT requirement for vessel

 To: materials-welding@googlegroups.com

 Date: Monday, August 31, 2015, 9:36 PM



 No. Since its a

 non-pressure part.

 On Aug 29, 2015 5:04 PM,

 "Prasad" <prsgne@gmail.com>

 wrote:

 Construction Code ASME Sec. VIII

 Div. 1 Edn. 2013



 Non pressure Part skirt support



 of vertical vessel not welded directly to vessel.



 MOC IS 2062 P no.1 Group  1



 Thk. 40 mm



 No special service requirement.







 For this case whether PWHT is mandatory?







 Regards,



 Prasad G.







 --



 You received this message because you are subscribed to
the

 Google Groups "Materials & Welding"
group.



 To unsubscribe from this group and stop receiving
emails

 from it, send an email to materials-welding+unsubscribe@googlegroups.com.



 To post to this group, send email to materials-welding@googlegroups.com.



 Visit this group at http://groups.google.com/group/materials-welding.



 To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d725eb3d-aca0-435c-ba4c-feadeba7f303%40googlegroups.com.



 For more options, visit https://groups.google.com/d/optout.











 --



 You received this message because you are subscribed to
the

 Google Groups "Materials & Welding"
group.



 To unsubscribe from this group and stop receiving
emails

 from it, send an email to materials-welding+unsubscribe@googlegroups.com.



 To post to this group, send email to materials-welding@googlegroups.com.



 Visit this group at http://groups.google.com/group/materials-welding.



 To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BEkGZc7hH9jjr5xvft3Oyfx3XYxTQ1Pc-7xwuD_KFs-Sj3DKQ%40mail.gmail.com.



 For more options, visit https://groups.google.com/d/optout.





--

You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.

To post to this group, send email to materials-welding@googlegroups.com.

Visit this group at http://groups.google.com/group/materials-welding.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1441302561.90531.YahooMailBasic%40web142701.mail.bf1.yahoo.com.

For more options, visit https://groups.google.com/d/optout.





--

You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.

To post to this group, send email to materials-welding@googlegroups.com.

Visit this group at http://groups.google.com/group/materials-welding.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEi5r3ajrjmpLYHNcFa%2BR4qRVjeJw7Je_5%2B-s6wY-MGzSWambw%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1441558198.11278.YahooMailBasic%40web142702.mail.bf1.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...