Tig rods are not needed to be vacuum packed since it does not contains flux/coatings which attracts moisture.

Regards

Dhevendran

On 6 Sep 2015 09:38, "ashok rai" <ashokr205@gmail.com> wrote:
Dear Experts,

As a corollary to this, is there any need to vacuum pack any TIG Welding Rods?

Ashok Rai

On Saturday, September 5, 2015 at 11:44:13 AM UTC+5:30, Jay Poojary wrote:

Dear Experts,

Can anybody from our experts,  share some information regarding vacuum pack low hydrogen electrode. Specially about the baking of this electrodes,  if left out.

Thanks & regards,
Jay Poojary,
QA/QC ENGINEER
OCLLC,
NIGERIA

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/33eecbe1-c5dc-4540-b475-923330483752%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGdQX6x_dPNZdi01daEef2SwcPAFjzjHxRT%3Dqj_WMHXGidZZBw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...