Thursday, September 3, 2015

Re: [MW:23389] PWHT requirement for vessel

Is their any reference to code that says PWHT not required for non pressure parts. Or only pressure parts required PWHT.

Regards,
Prasad G.

On 31 Aug 2015 19:55, "S.Mohammed" <mohd52100@gmail.com> wrote:
vessel subject to pwht then weld prior n do pwht.

bcse any way skirt going to weld with pad which directly weld with vessels.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/38b09431-d6ff-43a2-ad04-3bbecd11b648%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEi5r3YGXuXBPzZ3RCS-F%3DPhgSq3GVKFxcww8MnVFN_9E1wCwg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...