Tuesday, September 1, 2015

Re: [MW:23376] Orbital Tug welding in Cu Ni.

We have a brosure by Polysoude,the manufacturer. But the limitations are wide. Be cos the manufacturer parameters are commonly used for all material.

But everybody know about the parameters are related with position,size,thickness,metals, layers.

Anybody doing with the polysoude orbital machine, share the news about there.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b4540d14-3992-4758-97c3-8ac87a0cde21%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35742] PQR- Chemical testing requirements

Good Day to all, Reference std: ASME SEX IX Material ASTM A106 Gr B Pipe Dia and thickness: 2" and 8.74 mm. Service Fluid: Normal fluid...