Tuesday, September 15, 2015

[MW:23481] Re: SURFACE DEFECT IN HOT ROLLED PLATES

Knowing the steel grade and plate condition (hot rolled, normalized, et cetera) will help in being more accurate in describing the conditions. Conditions in first 2 photos (10-47-54 and 10-48-04) look like remants from scale patches, where the relatively light mill scale was rolled into the surface and then came off, leaving the mottled surface appearance. The last photo (22222) looks like rolled in scale, where heavier mill scale has been rolled into the plate surface leaving the surface imperfections, with some of the scale having  "popped out" leaving depressions in the plate surface.

On Monday, September 14, 2015 at 3:38:50 AM UTC-4, Mehdi Vafakhah wrote:
Dear experts

Could you help me to identify the these defect. ( attached pictures )

or refer a guide document that provide me more information about hot rolling defects.

best regards.

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ea4740c0-fb53-4ca4-8e94-4964e6af9997%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...