[MW:23475] Hydro test B31.3 345.4.2 (c)


Dear all,

Would appreciate if somebody clarify with example,

for me both paragraph same meaning because both the paragraph contain 1.5 test pressure??

(c) if the test pressure as defined above would produce
a nominal pressure stress or longitudinal stress in
excess of the yield strength at test temperature or a
pressure more than 1.5 times the component rating at
test temperature,

the test pressure may be reduced to
the maximum pressure that will not exceed the lesser
of the yield strength or 1.5 times the component ratings
at test temperature.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4a930648-e312-4659-86a5-472db9ac44dd%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...