[MW:23378] DN 80 Carbon steel pipe

Dear Experts,

I have a 80 mm dia pipe. I have done its wet chemical analysis according to IS228. The result shows as below,

C - 0.06
Si - 0.55
Mn - 0.45
P - 0.024
S - 0.023

I checked standard IS 1239. As per this standard, the chemical composition should be (all max), C - 0.2, Mn - 1.3, S&P - 0.04%.

My question is, can I say my pipe is IS 1239 pipe?

Please suggest what grade is my pipe?

Thank you.

Sincerely,
Abdulkadar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ef3fedae-c74f-45ea-943f-2a10ab38ffd8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...