Hi
Due to variation in Charpy V notch Impact values most of client specs. restrict the use of FCAW process in process equipments.
You can check your project specs. and decide.
Regards
Prem Nautiyal
9769316004
On Tuesday, July 1, 2014 1:30 PM, veera raghava kommisetti <kommisetti@gmail.com> wrote:
No Prohibition for use of FCAW from code.
But many client specification prohibit use of FCAW on Pressure Vessels.
On Tue, Jul 1, 2014 at 7:00 AM, Mhaskar Aly <mhaskar.aly@gmail.com> wrote:
--Dear Friends,We have· FCAW filler wire E71T-1C (Impact tested @ -20°C as per MTC)· Vessel (SA516 Gr 70; MDMT -29°C; Impact test exempted)Can we use this filler wire for welding on above vessel for:1. Nozzle to Shell weld2. RF Pad to Shell weld3. Vessel external Attachments with pad.\4. Saddle Pad to Shell weldKindly provide Code ReferenceThanks & regardsAli Mhaskar,
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment