Saturday, February 8, 2014

Re: [MW:20046] Query for HT condition for 50Ton Ranshorn Hook MOC: 20C15

Heattreatment Quenching and tempering is acceptable provided required hardness n microstructure is achieved

On Feb 7, 2014 7:09 PM, "Raghuram Bathula" <raghurambathula@gmail.com> wrote:

You need the hook as per IS 4367 or 5749? Why use both codes?

On Feb 7, 2014 9:33 PM, "D'Souza Bosco (Mumbai - Piping)" <B.A.Dsouza@ticb.com> wrote:
Material of Construction of 50 Ton hook: 20C15 complying to IS 4367 code, implies final condition Harden & Tempered.
Hook designed as per Ramshorn hook IS 5749-1970 calls for Normalizing heat treatment after forging and before testing.
A vendor has conducted Normalizing + Hardening (quenching) + tempering followered by testing.
 
Now the Inspection Agency is not accepting the Hook, on the basis that the hook is Q+T.
 
Has anyone experience in the above.
 
 
 
Thank You,
 
Regards,
Bosco A. D’Souza
Welding Engineer
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...