Hi
In AWS D1.1 there is no grouping of material in terms of P No. It is group no. only.
However for welder qualification the group no. is no a essential variable. The essential variable is F No.
Hope this clarifies your doubt.
Sent from Samsung Mobile
-------- Original message --------
From: Original Man
Date:05/02/2014 17:03 (GMT+08:00)
To: materials-welding@googlegroups.com
Subject: [MW:20016] Welder group no.(P No.) qualification limitations
Deal all
Please give me the code reference for Welder group no.(P No.) qualification limitations in AWS D1.1
-- Please give me the code reference for Welder group no.(P No.) qualification limitations in AWS D1.1
Thanks.
Adisak
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment