[MW:20020] Plating thickness and thread tolerance

Sirs,

If we have a shear bolt M10x1.25 4h with cadmium plating thickness varying
from 5 to 8 microns, what should be the tolerance of GO and NO gauge to be
used to check PCD before plating? What is the standard for this?

Regards

Mohan
VSSC



**Print this e-mail only if absolutely necessary. Save paper and keep India Green**

***The information contained in this e-mail message and / or attachments to it may contain confidential or privileged information. If you are not the intended recipient and received this e-mail in error, please notify us by reply e-mail / telephone and delete the message and attachments permanently. Thank you.***

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...