Re: [MW:17955] Measurement of interpass temperature

You can measure interpass temperature at locations about one inch on both sides of
 weld seam, at three different locations, at 120 degrees mutually.



From: sevak hiren <hirensevak80@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, June 17, 2013 5:24 PM
Subject: [MW:17950] Measurement of interpass temperature

Dear Experts,
 
Can anybody explain at which location interpass temperature to be measured during welding ?
 
Also what diference it will make in the weld metal property if we follow the wrong location of measurement of interpass temperature ? 
 
Is it written in any where in any code, where interpass temperature to be measured ?
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...