Saturday, February 2, 2013

Re: [MW:16680] tubes 25% Cr - 35% Ni and stabilizers of niobium and titanium

Mr. FJGV,

Enclosing certain details on 25Cr - 35 Ni of Ni & Ti stabilized steel, which I hope should be useful to you.

If U need any further info. please come back.

C Sridhar.


From: Francisco Javier Galvan Villagomez <fjgalvan@imp.mx>
To: materials-welding@googlegroups.com
Sent: Thursday, 31 January 2013 12:54 AM
Subject: [MW:16639] tubes 25% Cr - 35% Ni and stabilizers of niobium and titanium

It is possible do me get information from material tubes 25% Cr - 35% Ni and stabilizers of niobium and titanium for service in a hydrogen reformer .
 
aggrades your attention .
 
Ing. Francisco Javier Galván Villagómez.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...