Dear SirPlease find the below for Blind flange attachments calculation.Refer ASME Sec V111 Div -1 UG -34.UG-34 UNSTAYED FLAT HEADS AND COVERS
The minimum thickness of unstayed flat heads,
cover plates and blind flanges shall conform to the requirements
given in this paragraph. These requirements apply to both circular and noncircular
20 heads and covers.
The minimum required thickness of flat unstayed circular heads, covers and blind flanges shall be calculated by the following formula
t=p d CP / SE
Regards
Afroz
Dear friends,
Please guide. how blind flange made of plate material like A516-70 etc
are selected for specified rating like 150# , 300# for specified
Design pressure? Thanks in advance.
Best Regards
Aslam
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment